| Sieve size (mm) | 16 | 13.2 | 9.5 | 4.75 | 2.36 | 1.18 | 0.6 | 0.3 | 0.15 | 0.075 |
| Lower-upper limits (%) | 100 | 90–100 | 68–85 | 38–68 | 24–50 | 15–38 | 10–28 | 7–20 | 5–15 | 4–8 | Passing ratio (%) | 100 | 96.3 | 76.8 | 49.2 | 34.6 | 24.7 | 19.2 | 12.6 | 11.0 | 5.7 |
|
|