| Specimen | Direction | Initial cracking | Yielding of main rebar | Ultimate state | (mm) | (kN) | (mm) | (kN) | (mm) | (kN) |
| PC1 | Positive | 4 | 64.45 | 7.58 | 166.95 | 9.97 | 188.68 | Negative | 4 | 75.59 | 6.12 | 99.92 | 8.40 | 119.22 |
| PC2 | Positive | 2 | 69.67 | 8.43 | 192.27 | 10.03 | 207.13 | Negative | 4 | 79.96 | 6.56 | 119.56 | 8.44 | 132.26 |
| PC3 | Positive | 4 | 112.09 | 9.75 | 208.49 | 14.47 | 234.92 | Negative | 4 | 100.91 | 8.48 | 163.92 | 11.50 | 186.17 |
|
|