Findings of SCC in its fresh state.
| Mix ID | Fresh SCC characteristics | Slump flow (mm) | J-ring (mm) | L-box data | V-funnel (s) | Air content (%) | Relative density (kg/m3) |
| E0 | 741 | 721 | 1.20 | 8.6 | 3.45 | 2503 | E1 | 730 | 693 | 1.08 | 9.23 | 3.46 | 2513 | E2 | 716 | 679 | 1.04 | 10.13 | 3.47 | 2516 | E3 | 690 | 662 | 0.97 | 10.87 | 3.47 | 2517 | E4 | 739 | 715 | 1.20 | 9.52 | 3.47 | 2515 | E5 | 728 | 695 | 1.13 | 9.77 | 3.46 | 2513 | E6 | 705 | 673 | 1.03 | 9.86 | 3.46 | 2509 | E7 | 751 | 729 | 1.20 | 9.01 | 3.45 | 2506 | E8 | 738 | 717 | 1.20 | 9.31 | 3.44 | 2496 | E9 | 727 | 699 | 1.13 | 9.42 | 3.43 | 2489 |
|
|