Research Article
Crack Initiation, Propagation, and Coalescence Experiments in Sandstone Brazilian Disks Containing Pre-Existing Flaws
Figure 5
Geometry of pre-cracked specimens with different inclination angles: β = 0, 15°, 30°, 45°, 60°, 75°, and 90°.