Experimental Study on the Saturated Compacted Loess Permeability under K0 Consolidation
Figure 7
Relationship between the saturated permeability coefficient and the consolidation confining pressure. (a) Initial dry density ρd = 1.40 g/cm3. (b) Initial dry density ρd = 1.50 g/cm3. (c) Initial dry density ρd = 1.60 g/cm3. (d) Initial dry density ρd = 1.70 g/cm3.