Research Article

Strength Characteristics of Cement Treated and Expanded Polystyrene Mixed Lightweight of Waste Soil from the Construction Site of a Yangtze River Bridge in China

Table 4

The CU test scheme.

Waste soilMuddy clayFine sand

Vs : VE50 : 50 and 45 : 55
αc (%)14 and 16
Tc (curing time, d)7, 14 and 28
σ3 (cell pressures, kPa)50, 100 and 200