Research Article
Physical and Mechanical Properties of Gypsum-Like Rock Materials
Table 3
Tensile strength of remolded sample of high-strength gypsum power.
| No. | Rt (MPa) |
| Natural | A9 | 3.858 | A10 | 3.939 | A11 | 3.76 | Water saturation | C9 | 1.452 | C10 | 1.53 | C14 | 1.467 | 220°C high-temperature dehydration | D9 | 0.142 | D10 | 0.262 | D11 | 0.215 |
|
|