The compressive strength of fired shale hollow block.
| No. | Compressive strength (MPa) | Average value (MPa) | Coefficient of variation (%) |
| CB1 | 6.84 | 5.55 | 15.55 | CB2 | 6.08 | CB3 | 4.69 | CB4 | 5.98 | CB5 | 6.07 | CB6 | 5.24 | CB7 | 6.53 | CB8 | 4.43 | CB9 | 5.10 | CB10 | 4.53 |
|
|