Experimental Study on Cumulative Damage Behavior of Steel-Reinforced Concrete Columns
Figure 3
Failure mode of specimens. (a) SRC4 (1.5%). (b) SRC4 (2.0%). (c) SRC4 (2.5%-1st). (d) SRC4 (2.5%-6th). (e) SRC4 (2.5%-10th). (f) SRC4 (failure). (g) SRC1. (h) SRC2. (i) SRC3. (j) SRC1-2. (k) SRC4-2.