Research Article
Piezoresistivity of Cement Matrix Composites Incorporating Multiwalled Carbon Nanotubes due to Moisture Variation
Table 4
Average weight loss of specimens.
| Test number | 1 | 2 | 3 | 4 | 5 |
| Mass loss of CM | 0 | 0.75% | 1.57% | 2.18% | 3.29% | Mass loss of WCM1 | 0 | 0.67% | 1.58% | 2.25% | 3.36% | Mass loss of WCM3 | 0 | 1.12% | 1.91% | 2.54% | 3.11% |
|
|