Combined Effects of Graphite Tailings and Curing Conditions on the Early-Age Performances of Cement Mortar
Table 7
Porosity, total pore size, and area of GTCM-0 and GTCM-20 under SC and HWC methods.
| Age (d) | Specimen number | Curing scheme | Porosity (%) | Total intrusion volume (mL/g) | Total pore area (m2/g) |
| 1 | GTCM-0 | SC | 19.1284 | 0.097 | 11.162 | HWC | 14.9371 | 0.075 | 13.134 | GTCM-20 | SC | 19.0719 | 0.097 | 11.086 | HWC | 14.7349 | 0.073 | 13.112 | 3 | GTCM-0 | SC | 16.4691 | 0.0839 | 15.068 | HWC | 12.2389 | 0.0607 | 14.723 | GTCM-20 | SC | 16.3607 | 0.0723 | 11.794 | HWC | 12.0793 | 0.0602 | 9.828 |
|
|