Research Article
Properties and Applications of a New Chemical Grouting Material
Table 12
Compressive strength of trial lot before and after grouting.
| Order number | Sections | Invert (MPa) | Packed layer (MPa) | Track bed (MPa) | Before grouting | After grouting | Before grouting | After grouting |
| 1 | K251 + 025 | 25.8 | 18.8 | 26.0 | 41.7 | 43.0 | 2 | K251 + 060 | 24.8 | 18.7 | 25.8 | 43.7 | 44.5 | 3 | K251 + 190 | 24.6 | 19.0 | 26.5 | 44.5 | 44.8 | 4 | K251 + 217 | — | 8.8 | 26.2 | — | 42.3 | 5 | K251 + 227 | 25.3 | 13.9 | 25.4 | 18.9 | 42.8 | 6 | K251 + 260 | 26.2 | 18.8 | 25.9 | 43.3 | 43.9 | Design strength | 25 | 25 | 40 |
|
|