Review Article
Thermal and Mechanical Properties of Geopolymers Exposed to High Temperature: A Literature Review
Table 5
Stress-strain curves for different geopolymers at room temperature.
| Samples | M1 | M2 | M3 |
| Peak stress (MPa) | 60 | 46 | 39 | Peak strain (mm/mm) | 0.0038 | 0.0041 | 0.0035 | Variation trend after peak stress | Stress drops rapidly | Stress drops rapidly | Stress decreases slowly |
|
|