Research Article

Mechanism of Alkali-Activated Copper-Nickel Slag Material

Figure 7

SEM micrographs of CNSCMs with different SS contents and curing time of 28 (d). (a) Copper-nickel slag, (b) 6%, (c) 8%, and (d) 10%.
(a)
(b)
(c)
(d)