Research Article
Evaluating the Resistance Performance of the VAEPC and the PAFRC Composites against a Low-Velocity Impact in Varying Temperature
Table 8
Failure pattern of the specimens.
| Temperature condition (°C) | No. of spec. | PAFRC | VAEPC | Plain mortar | Front | Rear | Front | Rear | Front | Rear |
| −70 | 1 | | | | | | | Scabbing | Perforation | Perforation | 2 | | | | | | | Scabbing | Perforation | Perforation | 3 | | | | | | | Scabbing | Perforation | Perforation | 70 | 1 | | | | | | | Penetration | Perforation | Perforation | 2 | | | | | | | Penetration | Perforation | Perforation | 3 | | | | | | | Penetration | Perforation | Perforation | 140 | 1 | | | | | | | Perforation | Perforation | Perforation | 2 | | | | | | | Perforation | Perforation | Perforation | 3 | | | | | | | Scabbing | Perforation | Perforation |
|
|