The relation between deflections and strain and fatigue loading times for a bonded steel-plate-reinforced plate under the 200 kN load.

Fatigue cycles (104)Y-5 (με)Y-1 (με)W-1/2 (mm)

0216.5−217.91.11
50225.7−241.31.18
100241.6−260.11.28
150253.1−290.31.35
200258.3−325.61.43

Note. W-1/2: midspan deflection, Y-1: compressive strain at the top of the midspan, and Y-5: tension strain at the bottom of the midspan.