Research Article
Study on Fatigue Characteristics of Carbonation Erosion Prestressed Hollow Slabs in Whole Life Cycle
Table 15
Trend of dynamic displacement of test plates under 2 million fatigue cycles.
| Degree of erosion | Reinforcement method | Crest (mm) | Trough (mm) | Amplitude (mm) |
| Not eroded | Carbon fiber cloth | 0.39 | −0.32 | 0.71 | Not eroded | Sticky steel plate | 0.37 | −0.33 | 0.71 | Carbonization | Carbon fiber cloth | 0.53 | −0.52 | 1.05 | Carbonization | Sticky steel plate | 0.52 | −0.51 | 1.03 |
|
|