Research Article
Study on Fatigue Characteristics of Carbonation Erosion Prestressed Hollow Slabs in Whole Life Cycle
Table 17
Trend of modal of test plates under different fatigue cycles.
| Degree of erosion | Reinforcement method | 0 million cycles | 0.5 million cycles | 1 million cycles | 1.5 million cycles | 2.0 million cycles |
| Not eroded | Carbon fiber cloth | 4.8 | 3.1 | 2.7 | 2.7 | 2.3 | Not eroded | Sticky steel plate | 5.2 | 3.4 | 2.9 | 2.7 | 2.5 | Carbonization | Carbon fiber cloth | 5 | 3.1 | 2.9 | 2.7 | 2.4 | Carbonization | Sticky steel plate | 5.3 | 3.5 | 3 | 2.8 | 2.6 |
|
|