Research Article
Study on Fatigue Characteristics of Carbonation Erosion Prestressed Hollow Slabs in Whole Life Cycle
Table 9
The comparison of strain and deflection (before and after carbon-fiber reinforcement) under different load.
| Before reinforcement | After reinforcement | Load (kN) | W-1/2 (mm) | W-1/4 (mm) | Y-1 (με) | Y-5 (με) | W-1/2 (mm) | W-1/4 (mm) | Y-1 (με) | Y-5 (με) |
| 50 | 0.37 | 0.3 | −92.3 | 65.5 | 0.27 | 0.21 | 60.2 | 60.2 | 100 | 0.52 | 0.41 | −171.1 | 115.9 | 0.46 | 0.37 | 107.5 | 107.5 | 150 | 1.18 | 0.74 | −247 | 170.3 | 0.80 | 0.64 | 152.3 | 152.3 |
|
|