Research Article

Effects of Water and scCO2 Injection on the Mechanical Properties of Granite at High Temperatures

Figure 5

Postfailure images of tested granite specimens. From left to right, the experimental temperature conditions are 60°C, 90°C, 120°C, and 150°C. From top to bottom, the fluid injection conditions are dry, water, and CO2. The red lines show the fractures on the surface of tested specimens.