Research Article
Effect of Repeated Wetting-Drying-Freezing-Thawing Cycles on the Mechanic Properties and Pore Characteristics of Compacted Loess
Table 4
Results of the direct shear test for compacted loess specimens.
| Number of cycles | Shear strength (kPa) | Cohesion (kPa) | Internal friction angle (°) | 50 kPa | 100 kPa | 150 kPa | 200 kPa |
| 0 | 83.05 | 123.05 | 155.30 | 200.50 | 44.3 | 37.6 | 1 | 72.89 | 116.43 | 158.65 | 187.31 | 37.5 | 36.3 | 3 | 68.62 | 95.60 | 130.62 | 177.77 | 27.5 | 36.0 | 5 | 68.71 | 92.85 | 148.44 | 172.86 | 29.2 | 37.7 |
|
|