Advances in Civil Engineering / 2020 / Article / Fig 17

Research Article

Deterioration of the Internal Structure of Loess under Dry-Wet Cycles

Figure 17

CT images of the b section position of the LC-2 sample with cycle amplitude  = 20%. (a) Zero cycles. (b) One cycle. (c) Two cycles. (d) Four cycles. (e) Six cycles.