Mechanical Properties and Drying Shrinkage Investigation of Alkali-Activated Mortar Using Waste Glass Powder
Table 2
The mix-design proportions (kg/m3).
| Item | Water (H2O) | WGP | Quartz sand | SP | SF | NS | Sodium silicate | NaOH |
| A0 | 308.4 | 289.1 | 963.8 | 674.7 | 0 | 0 | 228.7 | 37 | S1 | 308.4 | 289.1 | 963.8 | 626.5 | 48.2 | 0 | 228.7 | 37 | S2 | 308.4 | 289.1 | 963.8 | 578.3 | 96.4 | 0 | 228.7 | 37 | S3 | 308.4 | 289.1 | 963.8 | 530.1 | 144.6 | 0 | 228.7 | 37 | S4 | 308.4 | 289.1 | 963.8 | 481.9 | 192.8 | 0 | 228.7 | 37 | S5 | 308.4 | 289.1 | 963.8 | 433.7 | 241 | 0 | 228.7 | 37 | NS1 | 308.4 | 289.1 | 963.8 | 655.4 | 0 | 19.3 | 228.7 | 37 | NS2 | 308.4 | 289.1 | 963.8 | 636.1 | 0 | 38.6 | 228.7 | 37 | NS3 | 308.4 | 289.1 | 963.8 | 616.9 | 0 | 57.8 | 228.7 | 37 | NS4 | 308.4 | 289.1 | 963.8 | 597.6 | 0 | 77.1 | 228.7 | 37 | NS5 | 308.4 | 289.1 | 963.8 | 578.3 | 0 | 96.4 | 228.7 | 37 |
|
|