Research Article

A Modified Cubic Law for Rough-Walled Marble Fracture by Embedding Peak Density

Figure 1

Test device and preparation of samples. (a) Self-made splitting mold; (b) marble fracture surfaces and single-fractured samples; (c) 3D laser scanning device; (d) 3D morphology of sample M1 upper fracture; (e) 3D morphology of sample M1 lower fracture.