Research Article
Strain Accumulation in Soft Marine Clay due to One-Way Cyclic Load with Variable Confining Pressure
Table 2
Scheme of CCP and VCP tests.
| Number of tests | p´0 (kPa) | qampl (kPa) | CSR | ηampl | Number of load cycles |
| D01 | 100 | 15 | 0.208 | 3 | 3000 | D02 | 100 | 15 | 0.208 | 1.0 | 3000 | D03 | 100 | 15 | 0.208 | 0.5 | 3000 | D04 | 100 | 20 | 0.278 | 3 | 3000 | D05 | 100 | 20 | 0.278 | 1.0 | 3000 | D06 | 100 | 20 | 0.278 | 0.5 | 3000 | D07 | 100 | 20 | 0.278 | 0.4 | 3000 | D08 | 100 | 20 | 0.278 | 0.3 | 3000 | D09 | 100 | 25 | 0.347 | 3 | 3000 | D10 | 100 | 25 | 0.347 | 1.0 | 3000 | D11 | 100 | 25 | 0.347 | 0.5 | 3000 | D12 | 100 | 35 | 0. 486 | 3 | 3000 | D13 | 100 | 35 | 0.486 | 1.0 | 3000 | D14 | 100 | 35 | 0.486 | 0.5 | 3000 | D15 | 100 | 35 | 0.486 | 0.4 | 3000 | D16 | 100 | 45 | 0.625 | 3 | 3000 | D17 | 100 | 45 | 0.625 | 1.0 | 3000 | D18 | 100 | 45 | 0.625 | 0.5 | 3000 | D19 | 100 | 55 | 0.764 | 3 | 3000 | D20 | 100 | 60 | 0.833 | 3 | 3000 | D21 | 100 | 65 | 0.903 | 3 | 3000 |
|
|