Research Article

Study on Cracking Resistance of Basalt Fiber-Reinforced Microbond Asphalt Macadam

Table 4

Performance indices and test results of basalt fibers.

Test itemTechnical requirementMeasured value

Breaking strength (MPa)≥1,5002325
Elongation at break (%)≤3.12.58
Oil absorption rate (%)≥5051.1
Combustible content (%)0.1∼1.00.5
Water content (%)≤0.20.08
Heat resistance-break strength retention (%)≥8592

The heat resistance is defined as the break strength retention after 4 h of continuous heating in an oven at 250°C.