Research Article
Micromechanical Properties of Steel-Fiber-Reinforced Cementitious Composites Characterized with Nanoindentation
Figure 9
Indentation hardness with distance from the steel-fiber surface at different silica fume contents and water-binder ratios. (a) Water-binder ratio of 0.18. (b) Water-binder ratio of 0.21. (c) Water-binder ratio of 0.24.
(a) |
(b) |
(c) |