Micromechanical Properties of Steel-Fiber-Reinforced Cementitious Composites Characterized with Nanoindentation

Table 5

Wt and η at different water-binder ratios when silica fume content was 0%.

SampleWt (10−9 J)We (10−9 J)Wp (10−9 J)η = We/Wt (%)
ITZCement matrixITZCement matrixITZCement matrixITZCement matrix

WB24SF008.0812.411.702.986.389.4320.9924.02
WB21SF009.5313.742.033.587.5010.1621.3526.05
WB18SF009.7918.862.305.497.4913.3723.5129.12