Research Article

Laboratory Study on Changes in Gas Desorption Properties of Anthracite after Cyclic Loading

Table 4

Fit results for the relationship between the desorption capacity of the briquette samples within 2.64 min and the square root of time under different loading frequencies.

Loading conditions0.5 MPa1.0 MPa1.5 MPa
Frequency (Hz)Amplitude (MPa)A1R2A2R2A3R2

412–182.76350.99692.61600.99843.08280.9951
73.60110.99463.67420.99453.71560.9939
103.98550.99384.05100.99084.01280.9938
152.47680.99622.15880.99652.63010.9875