Fitting results for the relationship between the desorption capacity of the briquette samples within 2.5 min and the square root of time under different loading conditions.

Loading conditions0.5 MPa1.0 MPa1.5 MPa
Frequency (Hz)Amplitude (MPa)A1R2A2R2A3R2

710–201.98080.99932.00100.98842.55110.9894
12–183.60110.99463.67420.99453.71560.9939
14–163.36550.97213.24290.99564.01320.9915
152.47680.99622.15880.99652.63010.9875