The main properties of ceramic permeable brick.

IndexSplitting tensile strength (MPa)Permeability coefficient (cm/s)Frost resistance (%)BNPPorosity (%)

GB/T25993-2010Average value ≥ 4.5Minimum value ≥ 3.4≥2.0 × 10−2Strength loss rate ≤ 20≥65≥15
Ceramic brick5.34.73.1 × 10−248924.82

BPN, British Pendulum Number.