Risk Assessment and Prevention of Surface Subsidence under Buildings by Cemented Paste Filling and Strip Mining Methods: A Case Study
Table 1
Classification of damage to surface brick-concrete structures [
16].
| Damage level | Surface deformations | Curvatures (mm/m2) | Inclinations (mm/m) | Classification | Structural processing | Horizontal deformation (mm/m) |
| I | ≤2.0 | ≤0.2 | ≤3.0 | Negligible damage | No repair | Very slight damage | Light repair | II | ≤4.0 | ≤0.4 | ≤6.0 | Slight damage | Minor repair | III | ≤6.0 | ≤0.6 | ≤10.0 | Medium damage | Medium repair | IV | >6.0 | >0.6 | >10.0 | Severe damage | Heavy repair | Very severe damage | Demolition and construction |
|
|