Research Article
Measuring Compressive Strength Characteristics of Soil-Dobak-Glue Mixtures over Curing Time
Table 7
Change of compressive strength and water content with increasing curing time.
| Curing time (days) | SO | SL | SS | 3 | 7 | 28 | 3 | 7 | 28 | 3 | 7 | 28 |
| Compressive strength (kPa) | 285.9 | 321.0 | 362.0 | 318.7 | 404.3 | 411.3 | 169.6 | 803.7 | 1090.1 | Residual water content (%) | 2.65 | 1.79 | 1.60 | 4.37 | 2.82 | 2.52 | 7.39 | 1.70 | 1.12 |
|
|