Research Article
Study on the Applicability of Elastic Recovery (Resilience) Experiment for Asphalt-Rubber
Figure 8
AR binders with #20–80 CR in the experimental procedure for elastic recovery at 180°C. (a) AR with #20 CR, (b) AR with #30 CR, (c) AR with #40 CR, (d) AR with #60 CR, and (e) AR with #80 CR.
(a) |
(b) |
(c) |
(d) |
(e) |