Compaction test results.

Mixture proportionOptimum water content (%)Maximum dry density (g/cm3)
4681046810

ITSF19.329.389.519.632.1172.1232.1282.133
ITSF29.239.319.479.582.1152.1242.1312.137
ITSC19.089.209.279.382.0772.0822.0892.096
ITSC29.139.329.419.502.0722.0802.0862.091