C25 grade of concrete quantity per 1 m3 by volume for mix of concrete.

Cement content397 kg

Fine aggregate682.9 kg
Course aggregate1024.35 kg
Water/cement ratio0.55
Glass fiber0.25%, 0.50% and 0.75%