Study on Distribution Characteristics of Metro Stray Current and Evaluation of Cumulative Corrosion Effect
Table 2
Location and length parameters of rail insulation damage.
| Type | Insulation damage location (m) | Insulation damage length (m) |
| Damaged acceleration | 400–490 | 90 | Damaged at constant speed | 800–890 | 90 | Damaged at deceleration | 1100–1190 | 90 | 45 m damaged at acceleration | 422.5–467.5 | 45 | 180 m damaged at acceleration | 355–535 | 180 |
|
|