Research Article

Performance of Ladle Furnace Slag in Mortar under Standard and Accelerated Curing

Table 1

Mix composition of mortars for a single mix in a mixer machine as adopted in this study.

SlSample nameCement (gm)LFS (gm)Sand (gm)Water (gm)

1ML0 = control (no LFS)4501350225
2ML5R = 5% raw LFS427.522.5
3ML10R = 10% raw LFS40545
4ML15R = 15% raw LFS382.567.5
5ML20R = 20% raw LFS36090
6ML25R = 25% raw LFS337.5112.5
7ML50R = 50% raw LFS225225
8ML5S = 5% sieved LFS427.522.5
9ML10S = 10% sieved LFS40545
10ML15S = 15% sieved LFS382.567.5
11ML20S = 20% sieved LFS36090
12ML25S = 25% sieved LFS337.5112.5
13ML50S = 50% sieved LFS225225