Research Article
Effect of Elevated Temperature on the Properties of Self-Compacting Mortar Containing Nanomaterials and Zircon Sand
Figure 16
(a) SEM images of self-compacting mortars containing zircon sand and nanoparticles at 27°C, 200°C, and 400°C. (b) SEM images of self-compacting mortars containing zircon sand and nanoparticles at 600°C and 800°C.