Shrinkage and Mechanical Properties of Fibre-Reinforced Blast Furnace Slag-Steel Slag-Based Geopolymer
Table 3
Mix proportions of geopolymer mortars.
| Samples | Slag (%) | Steel slag (%) | Activator modulus | Activator concentration (%) | Water binder ratio | Binder sand ratio | Fibre content (%) |
| PVA-0 | 70 | 30 | 1.2 | 22 | 0.50 | 0.60 | 0 | PVA-1 | 70 | 30 | 1.2 | 22 | 0.50 | 0.60 | 0.1 | PVA-2 | 70 | 30 | 1.2 | 22 | 0.50 | 0.60 | 0.2 | PVA-3 | 70 | 30 | 1.2 | 22 | 0.50 | 0.60 | 0.3 | PVA-4 | 70 | 30 | 1.2 | 22 | 0.50 | 0.60 | 0.4 | BF-1 | 70 | 30 | 1.2 | 22 | 0.50 | 0.60 | 0.1 | BF-2 | 70 | 30 | 1.2 | 22 | 0.50 | 0.60 | 0.2 | BF-3 | 70 | 30 | 1.2 | 22 | 0.50 | 0.60 | 0.3 | BF-4 | 70 | 30 | 1.2 | 22 | 0.50 | 0.60 | 0.4 |
|
|