Crushing strength of concrete cylinder in 28 days.
| Si. no. | AWA (%) | Cement weight loss (%) | Slump (mm) | Cylinder crushing strength (28 days) (MPa) |
| 1. | 0.0 | 10.1 | 210 | 32.1 | 2. | 0.1 | 8.2 | 190 | 35.5 | 3. | 0.2 | 7.5 | 170 | 37.2 | 4. | 0.3 | 5.1 | 150 | 42.6 | 5. | 0.4 | 4.8 | 140 | 39.2 | 6. | 0.5 | 3.2 | 130 | 37.4 |
|
|