Research Article

Effect of SiO2 Methyl Modification on the Performance of Nondispersible Underwater Concrete and Reinforcement Mechanism

Table 6

Performance requirements of UWC.

Experimental projectsSpecific projectsParameter requirements

FluiditySlump (mm)230 ± 20
Slump flow (mm)450 ± 20

Antiwashout resistanceLoss of cement (g)<1.5
Suspended matter content (mg/L)<150
pH<12

Underwater/in-air strength ratio (MPa)7d>35
28d>50