Research Article
Postfire Residual Strength and Morphology of Concrete Incorporating Natural Rubber Latex Exposed to Elevated Temperatures
| S/N | Sample | Proportions |
| 1 | Control sample | Control sample containing no NRL | 2 | M1 | Sample containing 1% of NRL | 3 | M2 | Sample containing 1.5% of NRL | 4 | M3 | Sample containing 3% of NRL |
|
|