Synthesis and Optimization of MWCNTs on Co-Ni/MgO by Thermal CVD
Figure 1
CNT
yield as a function of (a) Co-Ni catalysts loading (Wt%) during 60 minutes growth
time with flow of H2 + C2H2 (100 + 15 mL/min) at
600°C, (b) reaction temperature of 25% Co + 25% Ni catalyst on MgO
support.