Research Article

Fabrication and Electrical Characterization of Translucent Bi12TiO20 Ceramics

Figure 5

(a) BTO ceramics sintered at 800°C/3 h and polished to the thickness of 0.5 mm. (b) Transmission spectra of the sample.
536754.fig.005a
(a)
536754.fig.005b
(b)