Alkali Cation Potential and Functionality in the Nanoporous Prussian Blue Analogues
Figure 6
(a) Current density () of ITO/Na0.72Ni[Fe(CN)6]0 : 68·5.1H2O (560 nm)/Na0.79Co[Fe(CN)6]0:90·2.9H2O (320 nm)/ITO device against time () under periodic rectangular voltage () on the M = Ni side. (b) curves at 0.6 V of the device before and after the K+-treatment.