Research Article

Photocatalytic Surface Modification of PI Film for Electroless Copper Plating

Table 3

The contents of carbon groups on the PI film surface before and after photocatalytic treatment (treatment time: 30 min, : 1.0 g/L).

UV powerC-C, C-H, C=C (%)C-O, C-N (%)N(C=O)2 (%) (%)-COOH (%)

053.738.714.82.80
100 W48.037.67.32.24.9
300 W46.538.36.82.36.1