Physical Structure Induced Hydrophobicity Analyzed from Electrospinning and Coating Polyvinyl Butyral Films
Figure 3
3D surface roughness of the prepared PVB films under spin-coating 250 r/s (a), bar-coating 6 μm (b), positive electrospinning 15 cm (c), and negative electrospinning 15 cm (d). The inset images showed the 2D surface roughness of these films.
(a) |
(b) |
(c) |
(d) |