(a) Magnetic tape 1/4-inch-wide with magnetic coating shedding (“a failure of the binder/oxide coating to adhere to the substrate film, resulting in the delamination—the peeling away—of one from the other” [32]). (b): Compact Disc exhibiting a longitudinal crack (“a break without physical separation” [19, Appendix C]).
276354.fig.005a
(a) Tape with magnetic coating shedding
276354.fig.005b
(b) Cracked Compact Disc