Plasma Treatment and TEOS Modification on Wood Flour Applied to Composite of Polyvinyl Chloride/Wood Flour
Table 1
Surface area and pore volume of original WF, plasma treated WF, and WS5.
| Sample | BET surface area (m2/g) | Micropore surface area (m2/g) | External surface area (m2/g) | Volume of pores (cm3/g) | Adsorption average pore width (nm) |
| Original WF | 0.7132 | 0.3479 | 0.3653 | 0.001805 | 50.01177 | Plasma treated WF | 0.7556 | 0.3463 | 0.4093 | 0.001992 | 45.72897 | WS5 | 0.7771 | 0.3678 | 0.4093 | 0.002074 | 47.59989 |
|
|